Multibase Nylex™ 2185 FR V0 Polyamide + PP

Category Polymer , Thermoplastic , Nylon , Polypropylene (PP)
Manufacturer Multibase
Trade Name Nylex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Nylex™ 2185 FR V0 Polyamide + PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing, Electrical Safety EquipmentInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM 792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.7 MPa
6200 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 42.7 MPa
6200 psi
ASTM D790
Flexural Modulus 1.52 GPa
220 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched 0.667 J/cm
1.25 ft-lb/in
ASTM D256
Gardner Impact 14.12 J
10.42 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C
201 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.8 °C
127 °F
Unannealed; ASTM D648
Vicat Softening Point 166 °C
331 °F
ASTM D1525
Flammability, UL94 V-0
V-0