Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.667 J/cm
1.25 ft-lb/in
ASTM D256
Multibase Nylex™ 2185 FR V0 Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric..
Izod Impact, Notched 0.667 J/cm
1.25 ft-lb/in
ASTM D256
Ovation Polymers RIGITRON 10020 GF Polycarbonate, 20% Glass Reinforced
PC - Glass reinforced (20 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared accor..
Izod Impact, Notched 0.667 J/cm
1.25 ft-lb/in
ASTM D256
Ovation Polymers RIGITRON 20433 GF PBT, 33% Glass Reinforced
PBT - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared acco..
Izod Impact, Notched 0.667 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.25 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Lubri-Tech™ AS-10GB/02S Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled  (discontinued **)<
Description/Features:Glass Bead FilledSilicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.667 J/cm
1.25 ft-lb/in
73°F, 0.125 in; ASTM D256
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Izod Impact, Notched 0.667 J/cm
1.25 ft-lb/in
ASTM D256
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Izod Impact, Notched >= 0.667 J/cm
>= 1.25 ft-lb/in
Method A; ASTM D 256
Karina E 854-35/9-A-ERYB Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched 0.667 J/cm
1.25 ft-lb/in
ASTM D256
Ecomass® 1700CO93 Copper Powder Filled Polyamide, Injection Molding
High Specific Gravity, Copper Powder Filled Polyamide (PA), Rigid, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInform..
Izod Impact, Notched 0.667 - 1.07 J/cm
1.25 - 2.00 ft-lb/in
ASTM D256
Buckeye Polymers BP RPPC 1020 TU BLK Polypropylene Copolymer
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis..
Izod Impact, Notched >= 0.667 J/cm
>= 1.25 ft-lb/in
ASTM D256
Buckeye Polymers BP RPPC 2010 CW Polypropylene, Calcium Filled
Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges fro..
Izod Impact, Notched 0.667 J/cm
1.25 ft-lb/in
ASTM D256
Aaron Industries AAROPRENE® TFIPP 2020 High Impact Talc Filled Polypropylene
AAROPRENE® TFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.