Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase SILASTIC® C7-4550 TBPB Dow-Corning Biomedical Grade ETR Elastomer

Category Polymer , Thermoset , Silicone
Manufacturer Multibase
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase SILASTIC® C7-4550 TBPB Dow-Corning Biomedical Grade ETR Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Multibase
Mechanical Properties Metric English Comments
Hardness, Shore A 48
48
as molded
50
50
post cured- 2 hours at 177°C
54
54
post cured- 4 hours at 204°C
Tensile Strength, Ultimate 10.3 MPa
1490 psi
post cured- 4 hours at 204°C
10.62 MPa
1541 psi
as molded
10.8 MPa
1560 psi
post cured- 2 hours at 177°C
Tensile Strength, Yield 2.86 MPa
415 psi
at 200%, as molded
3.07 MPa
445 psi
at 200%, post cured- 2 hours at 177°C
3.38 MPa
490 psi
200%, post cured- 4 hours at 204°C
Elongation at Break 514 %
514 %
post cured- 4 hours at 204°C
559 %
559 %
post cured- 2 hours at 177°C
596 %
596 %
as molded
Tear Strength 27.0 kN/m
154 pli
post cured- 2 hours at 177°C; Die B
28.4 kN/m
162 pli
post cured- 4 hours at 204°C; Die B
28.9 kN/m
165 pli
as molded; Die B
Copyright © lookpolymers.com All Rights Reserved