Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® 72A Butene Copolymer LLDPE Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer NOVA Chemicals
Trade Name Sclair®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 72A Butene Copolymer LLDPE Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
72A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. 72A is subject to the specific limitation that it may not be used in articles used for packing or holding food during cooking.NOVA Chemicals' polyethylene resins are chemically and biologically inert.Features: Good processability, Excellent impact resistance, Outstanding flexibility and warpage resistance, Good organoleptic properties and natural colorAdditives: AntioxidantApplications: Housewares, Flexible food packaging lids, Caps and closures, Compounding
Physical Properties Metric English Comments
Bulk Density 0.720 g/cc
0.0260 lb/in³
ASTM D 792
Density 0.924 g/cc
0.0334 lb/in³
ASTM D 792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D 2240
Tensile Strength at Break 9.00 MPa
1310 psi
50 mm/min test speed; ASTM D 638
Tensile Strength, Yield 12.4 MPa
1800 psi
50 mm/min test speed; ASTM D 638
Elongation at Break 550 %
550 %
50 mm/min test speed; ASTM D 638
Flexural Modulus 0.375 GPa
54.4 ksi
ASTM D 790
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 °C
198 °F
ASTM D 1525
Processing Properties Metric English Comments
Melt Temperature 170 - 215 °C
338 - 419 °F
Recommended
Users viewing this material also viewed the following: