Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 195 - 215 °C | 383 - 419 °F | |
SABIC 118 Series Linear Low Density Polyethylene for Blown Film Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st.. |
|||
Melt Temperature | 195 - 215 °C | 383 - 419 °F | |
SABIC 120W Linear Low Density Polyethylene for Blown Film Product Description: 120W is a Linear Low Density Polyethylene grade suitable for general purpose packaging. Films produced using this resin yield good tensile properties, impact strength and opti.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | Recommended |
NOVA Chemicals Sclair® 19C (High Gloss) HDPE Blow Molding Resin 19C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2909 HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughness, Good top loading capability, High surface glossApplications: Tote boxes, Beverage cratesAdditives: Antioxidant, Ultraviolet light stabilizersIn.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 56B4 HDPE Blow Molding Resin Extra-high stress crack resistance, Good processabilityApplications: Very high ESCR, Ideally suited for use in most food, pharmaceutical, households and industrial chemical applications, Little/no s.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 8107 UV8D Butene LLDPE Rotational Molding Resin Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin
(discontinued **) Features: Good processability, excellent impact resistance, excellent flexibility and freedom from warpage.Applications: Automotive splash-guards, large containers, closures and lids for food applic.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2607 HDPE Injection Molding Resin Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2709 HDPE Injection Molding Resin Features: Excellent cold temperature toughness, high stiffness.Applications: Housewares, containers, pails, closures.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 8405 BK, 8405GBK MDPE Rotational Molding Resin
(discontinued **) Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 8406 UV8D, 8406G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 8504 BK, 8504 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Low melt index, excellent ESCR, high toughness at low temperatures.Applications: Large chemical storage tanks.Data provided by the manufacturer. |
|||
Melt Temperature | 205 - 215 °C | 401 - 419 °F | |
Eastman Tenite 264-16 CAB Cellulose Acetate Butyrate
(discontinued **) 16% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | |
DuPont Elvax® 3190 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melt Temperature | 200 - 215 °C | 392 - 419 °F | |
Ecomass® 4450CI86 Carbonyl Iron Filled Polypropylene Nontoxic alternative to Lead (Pb), for shielding applicationsHigh Specific GravityCarbonyl Iron Filled Polypropylene Random Co-PolymerInformation provided by Technical Polymers |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | Blown/Cast Film Coextrusion |
DuPont™ Elvax® 3190A Ethylene Vinyl Acetate DuPont™ Elvax® 3190A is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3.. |
|||
Melt Temperature | 190 - 215 °C | 374 - 419 °F | Injection molding |
BASF Ultraform® N2640 Z2 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Melt Temperature | 190 - 215 °C | 374 - 419 °F | Injection-molding |
BASF Ultraform® N2650 Z4 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr.. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | |
Huntsman Rexell® V8402 Cast Film Extrusion LLDPE
(discontinued **) Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent mechanical strength, low sealing temperature, and good flex crack resistanceApplications: Sealing layer in.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2607-UV9 HDPE Injection Molding Resin
(discontinued **) Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids, housewares, deep skirt lids,.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 8306 BK, 8306G BK MDPE Rotational Molding Resin
(discontinued **) Features: Balanced combination of toughness, ESCR and processability.Applications: General purpose.Data provided by the manufacturer. |
|||
Melt Temperature | 182 - 215 °C | 360 - 419 °F | |
ExxonMobil Santoprene® 8271-80HT Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use. It can be processed using injection molding or extrusion melt pro.. |
|||
Melt Temperature | 190 - 215 °C | 374 - 419 °F | Injection molding |
BASF Ultraform® N2650 Z6 POM + PUR Description: Elastomer-modified injection molding grade for applications requiring highest impact strength together with low stiffness.Information provided by BASF |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | |
DuPont Elvax® 3190LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | |
DuPont Elvax® 3175LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2111 LLDPE Injection Molding Resin
(discontinued **) Good processability, Excellent impact resistance, Excellent flexibility and freedom from warpageApplications: Automotive splash-guards, Large containers, Closures and lids for food applicationsAddit.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2508-UV13 MDPE Injection Molding Resin
(discontinued **) Excellent processability for applications requiring stiffness and toughness, Good cold temperature impact propertiesApplications: Roll-out cart lidsAdditives: Elevated levels of ultraviolet light st.. |