NYCOA 1595 HS Impact Modified, Medium Viscosity Nylon 6 Resin

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer NYCOA, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA 1595 HS Impact Modified, Medium Viscosity Nylon 6 Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NYCOA 1595 HS is a medium viscosity Nylon 6 resin, which offers superior flexibility and toughness in both molding and extrusion applications. Its high melt viscosity and strength provides excellent processability and yields extremely tough and resilient finished articles. Injection molding of high strength parts can be accomplished with molding cycles almost equivalent to those obtained with general-purpose grade resins, even though higher cylinder temperatures may sometimes be required. NYCOA 1595 HS resin has acceptance in diversified applications from convoluted tubing, windshield washer tubing, profile, to tough molded articles.Information provided by Nycoa, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Water Absorption 1.7 %
1.7 %
24 hours; ASTM D570
Melt Flow 2.5 g/10 min

@Load 1.00 kg,
Temperature 235 °C
2.5 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Flexural Strength 60.0 MPa
8700 psi
ASTM D790
Flexural Modulus 1.60 GPa
232 ksi
ASTM D790
Izod Impact, Notched 5.00 J/cm
9.37 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D789