Nabaltec NABALOX® NO 135 Ground Alumina

Category Ceramic , Oxide , Aluminum Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Nabaltec GmbH
Trade Name NABALOX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nabaltec NABALOX® NO 135 Ground Alumina.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insulationhigh mechanical strengthhigh temperature propertiesdimensional accuracyoptimized chemical resistanceRefractory Industry, Wear-resistant ceramicsInformation provided by Nabaltec.
Physical Properties Metric English Comments
Bulk Density 0.750 g/cc
0.0271 lb/in³
Density 3.90 g/cc
0.141 lb/in³
Grain Size 5.0 µm
5.0 µm
Median
Specific Surface Area 0.80 m²/g
0.80 m²/g
BET
Component Elements Properties Metric English Comments
Al2O3 99.6 %
99.6 %
Fe2O3 0.030 %
0.030 %
Na2O 0.30 %
0.30 %
SiO2 0.030 %
0.030 %
Descriptive Properties Value Comments
a-Al2O3 Content % 98