Transparent polyimide with low moisture uptake and low dielectric constant. Transparent polyimide with low moisture uptake and low dielectric constant. LaRC™ CP1 exhibits the lowest moisture uptake, lowest dielectric constant, and lowest color of all commercially available polyimides, making it an ideal choice for electronics, displays, and aerospace applications. Additionally, continuous rolls are available now in thicknesses as low as 2.5 microns (0.1 mil) and in widths up to 60 inches (152 cm). Information Provided by NeXolve Corporation.
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792-08
Water Absorption 0.40 %

@Time 86400 sec
0.40 %

@Time 24.0 hour
ASTM D570-98
Mechanical Properties Metric English Comments
Tensile Strength 87.0 MPa

@Thickness 0.0250 mm
12600 psi

@Thickness 0.000984 in
ASTM D882-02
Elongation at Break 16 %

@Thickness 0.0250 mm
16 %

@Thickness 0.000984 in
ASTM D882-02
Modulus of Elasticity 2.00 GPa
290 ksi
ASTM D882-02
Thermal Properties Metric English Comments
CTE, linear 51.0 µm/m-°C

@Thickness 1.00 mm,
Temperature 125 - 175 °C
28.3 µin/in-°F

@Thickness 0.0394 in,
Temperature 257 - 347 °F
ASTM E831-06
Glass Transition Temp, Tg 263 °C
505 °F
DSC; ASTM E1356-03
Optical Properties Metric English Comments
Refractive Index 1.57

@Wavelength 549 nm
1.57

@Wavelength 549 nm
Abbe; ASTM D542-00
Haze 0.60 %

@Thickness 0.0250 mm
0.60 %

@Thickness 0.000984 in
ASTM D1003-11
Transmission, Visible 0.83 %

@Thickness 0.0250 mm
0.83 %

@Thickness 0.000984 in
Solar Transmittivity; ASTM E903-96
88 %

@Wavelength 400 - 780 nm,
Thickness 1.00 mm
88 %

@Wavelength 400 - 780 nm,
Thickness 0.0394 in
Average
UV Transmittance 50 %

@Thickness 0.0250 mm,
Wavelength 409 nm
50 %

@Thickness 0.000984 in,
Wavelength 409 nm
50% Transmission UV Cutoff
Emissivity (0-1) 0.45

@Thickness 1.00 mm
0.45

@Thickness 0.0394 in
Infrared (Hemispherical); ASTM E408-71
Reflection Coefficient, Visible (0-1) 0.090

@Thickness 0.0250 mm
0.090

@Thickness 0.000984 in
Solar Reflectivity; ASTM E903-96
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+9 ohm-cm
>= 1.00e+9 ohm-cm
ASTM D257-91
Surface Resistivity per Square >= 1.00e+12 ohm
>= 1.00e+12 ohm
ASTM D257-91
Dielectric Constant 2.4 - 2.5

@Frequency 1.00e+10 Hz
2.4 - 2.5

@Frequency 1.00e+10 Hz
Dielectric Strength 197 kV/mm
5000 kV/in
ASTM D149-09
Descriptive Properties Value Comments
Applications Composites
Displays
Electrical Insulation
Electronics
Insulation Blankets
Insulation Tubing
Optical Filters/Mirrors
Pressure Sensitive Tape
Spare Structures
Thermal Control
Characteristics 10 Year Rated Life in GEO
Conductive/Nonconductive Offerings
Highly Transparent
Low Dielectric Constant
Low Moisture Uptake
UV Resistant
Vacuum Coating Compatible
Solar Absorptivity 0.08
1 mil thickness; ASTM E903-96