Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.00 GPa | 290 ksi | ASTM D-638 |
Plaskolite Optix® CP - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | 50% RH |
Murtfeldt Murdopol® Nylon 12 Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ASTM D638 |
Plaskolite West Optix® CA-927 Impact Modified Acrylic Resin Injection Molding Grade Pellets. Better impact strength than CA-924. Excellent surface gloss, optical clarity, and practical toughness. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8210 Rigid Opaque Prototyping Polymer Primary material: VeroBlueSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the .. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8330 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ASTM D-638 |
Plaskolite Optix® CP - 927 G High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Modulus of Elasticity | 2.00 - 6.80 GPa @Temperature 60.0 - 150 °C |
290 - 986 ksi @Temperature 140 - 302 °F |
Average value: 4.78 GPa Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | |
Lehmann & Voss LUVOCOM® 1850-8197 PBT, lubricant modified, easy flowing, demolding aid Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | |
Lehmann & Voss LUVOCOM® 50-7317 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ISO 527-2 |
Tisan TISARBON® UNR Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 15MB400 OPP Film Product Description: Bicor 15MB400 is one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Ou.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 18MB090 OPP Film Product Description: Biaxially oriented polypropylene film metallizable on one side, with a slip controlled broad seal range surface on the other side. Once metalized, film designed to be used in la.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 20MB080 OPP Film Product Description: Bicor 20NB080 is a biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a s.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 20MB400 OPP Film Product Description: Bicor 20MB400 is a one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 20MB668 OPP Film Product Description: Bicor 20MB668 is a high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provid.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 25MB666 OPP Film Product Description: A Biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, .. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 29MB080 OPP Film Product Description: A biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a single web in HFFS.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 40MB668 OPP Film Product Description: A high speed transparent biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides excellent perfo.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 42MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent PP film, coated one side PVdC, one side acrylic, This film provides outstanding performance on all packaging machines.Availabi.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 40LL666 OPP Film Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Metallyte™ 15MM348 OPP Film Product Description: An enhanced barrier metalized film with a very broad seal range and can be considered a multipurpose film. This designed of this film allow excellent performance on HFFS machine.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM383 OPP Film Product Description: A biaxially oriented very high barrier metalized polypropylene film. This film offers an outstanding moisture barrier and a broad seal range surface on the other side. This film.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM488 OPP Film Product Description: A metalized biaxially oriented polypropylene film, metalized on one side. MM488 is typically used in laminates as the inner web for VFFS and HFFS applications. Due to its slip c.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ISO 178 |
Addiplast Addilene PMD 50306 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 1 Flame Retardant Nylon 66 Flame retardant, halogen freeInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.00 - 8.96 GPa | 290 - 1300 ksi | Average value: 3.93 GPa Grade Count:37 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Modulus of Elasticity | 2.00 - 6.00 GPa | 290 - 870 ksi | Average value: 2.67 GPa Grade Count:26 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |