Network Polymers 351 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers 351 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ignition RetardantInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4200 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 39.3 MPa
5700 psi
ASTM D790
Flexural Modulus 1.90 GPa
275 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
Injection Molding; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.1 °C
187 °F
ASTM D648
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Flammability, UL94 V-0
V-0
0.0625 in
Descriptive Properties Value Comments
Color Stability min 10
Change in E at 300 hours; ASTM D4459