Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Network Polymers 351 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 39.3 MPa | 5700 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Strength | 39.3 MPa | 5700 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Strength | 39.3 MPa | 5700 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Total PSI 830 Polystyrene Polystyrene 830 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. The high flow 830 material aids production of stress free parts.The m.. |
|||
Flexural Strength | 39.3 MPa | 5700 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Strength | 39.3 MPa | 5700 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Strength | 39.3 MPa | 5700 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Entec Hyrene® PS-HI 3/4 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Flexural Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Entec Hyrene® PS-HI 8/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Flexural Strength | 39.3 MPa | 5700 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers NPP25-1001 TF20 20% Talc Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Americas Styrenics STYRON® 478 High Impact Polystyrene Product CharacteristicsGood glossExcellent balance of flow and stiffnessFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsAppliancesMedicalHousewaresConsumer electronicsIn.. |