Description: Injection Molding Grade, High Melt FlowInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 200 °C
18 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 71
71
ASTM D785
Tensile Strength at Break 47.6 MPa
6900 psi
chs 2 in/min; ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Tensile Modulus 2.96 GPa
430 ksi
chs 2 in/min; ASTM D638
Izod Impact, Notched 0.133 J/cm
0.250 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Annealed; ASTM D648
Vicat Softening Point 93.0 °C
199 °F
ASTM D1525