Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers Nylon 6030

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers Nylon 6030.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Natural Nylon (33% Glass Fiber)Information provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 141 MPa
20500 psi
ASTM D638
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched >= 0.641 J/cm
>= 1.20 ft-lb/in
1/8 in specimen; ASTM D256
Thermal Properties Metric English Comments
Melting Point 249 °C
480 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 224 °C
435 °F
0.125 in bar; ASTM D648