NextGen Adhesives G907-21 Structural Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer NextGen Adhesives
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NextGen Adhesives G907-21 Structural Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NGAC G907-21 is a high viscosity and thixotropic adhesive system that is specifically formulated for structural bonding applications: industrial, electronics and aerospace.Advantages and Applications: The NGAC G907-21 is recommended for any application requiring a high fill adhesive will not sag, providing excellent adhesion and mechanical/structural strength. The NGAC G907-21 is easily mixed and cured at room temperature and provides excellent adhesion to glass, ceramic, metal and plastic.Information Provided by Nextgen Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
Solids Content 100 %
100 %
Viscosity 100000 cP
100000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Shear Strength 20.7 MPa
3000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg 110 °C
230 °F
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
Color Milky White
Mix Ratio by Weight (R/H) 100/22