Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Niche Polymer PPHT40BK Homopolymer PP, 40% Talc Fiber Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer Niche Polymer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niche Polymer PPHT40BK Homopolymer PP, 40% Talc Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00800 cm/cm
0.00800 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.7 MPa
4600 psi
ASTM D638
Elongation at Break 10.0 %
10.0 %
ASTM D638
Flexural Strength 51.0 MPa
7400 psi
ASTM D790
Flexural Modulus 3.30 GPa
479 ksi
ASTM D790
Izod Impact, Unnotched 0.200 J/cm

@Thickness 3.17 mm
0.375 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 174 °C
345 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 171 - 193 °C
339 - 379 °F
ASTM D789
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: