Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 51.0 MPa | 7400 psi | |
Plastcom SLOVALEN PH 49 GF 10 GB 20 PP, 20% glass beads, 10% glass fibre, coupling agent FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10 % glass fiber and 20% glass beads, contains themodifier of mechanical properties. Increased strength in comparis.. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ASTM D790 |
Niche Polymer PPHT20BK Homopolymer PP, 20% Talc Fiber Filled Information provided by Niche Polymer |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ASTM D790 |
Niche Polymer PPHT40BK Homopolymer PP, 40% Talc Fiber Filled Information provided by Niche Polymer |
|||
Flexural Strength | <= 51.0 MPa | <= 7400 psi | ISO 178 |
Polykemi AB POLYfill PPH T15020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 51.0 MPa | <= 7400 psi | ISO 178 |
Polykemi AB POLYfill PPH T16020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 51.0 MPa | <= 7400 psi | ISO 178 |
Polykemi AB POLYfill PPH T20020 UV Polypropylene Homopolymer, Mineral Reinforced, UV-Stabilized Information provided by Polykemi AB |
|||
Flexural Strength | <= 51.0 MPa | <= 7400 psi | ISO 178 |
Polykemi AB POLYfill PPH T3022D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON TE002 PU LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GC-0703 ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0170 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GC-0703 ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0170 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ASTM D638 |
Plastics Group Polifil® GFPP-10 10% Glass-Reinforced Polypropylene Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou.. |
|||
Flexural Strength | 51.0 MPa @Temperature 260 °C |
7400 psi @Temperature 500 °F |
ASTM D790 |
UBE UPIMOL® SA101 Heat-Resistant Polyimide Shape Description: UPIMOL® SA101 is an excellent heat-resistant polyimide shape, based on Biphenyl tetracarboxilic dianhydride(BPDA) originally developed by UBE. UPIMOL® SA101 has improved high durabili.. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ISO 178 |
Polyplastics Duracon® SF-15 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ISO 178 |
Polyplastics Duranex® CE7300 Polybutylene Terephthalate (PBT), Higher impact resistant DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ASTM D790 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-709S ABS - Extrusion Super Impact Extrusion |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ASTM D790 |
Denka STYROL MW1 Polystyrene "DENKA SYTROL MW" is a well-balanced polystyrene (PS) resin, with a high tensile strength as well as good moldability. Overturning the traditional understanding that PS resin is "hard and brittle," .. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ISO R178 |
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved Information provided by Arkema Group |
|||
Flexural Strength | 51.0 MPa | 7400 psi | |
BCC Products BC 7009-2 Epoxy Casting BC 7009-2 is an iron filled, low-cost mass casting system. Recommended for use in casting a minimum of two inches and a maximum of six inches in non-conductive molds. Thicknesses to nine inches in m.. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339M20CL Mica Reinforced Coupled |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ASTM D790 |
Americas Styrenics MC3700 High Heat Crystal Polystyrene Product CharacteristicsEasy filling of thin-walled partsExceptional mold releaseImproved cycle times in hard to fill partsFood Contact CompliantUL Classification 94HBUSP Class VITypical Applications.. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ASTM D790 |
Americas Styrenics STYRON® 649D High Heat Crystal Polystyrene Product CharacteristicsExcellent moldabilityExcellent gloss in coextrusionExcellent clarityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk .. |
|||
Flexural Strength | <= 51.0 MPa | <= 7400 psi | ISO 178 |
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ISO 178 |
Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable prot.. |
|||
Flexural Strength | 51.0 MPa | 7400 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON MFD03 PP LNP* STAT-KON* MFD03 is a compound based on Polypropylene resin containing 15% Glass Fiber. Added features of this material include: Electrically Conductive. |