Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nihon Superior SN100CL Lead-Free Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Nihon Superior
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nihon Superior SN100CL Lead-Free Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used for hot air solder leveling (HASL). Features include: Excellent fluidity; Bridge-free coating of the fine pitch circuitry; Bright smooth and uniform coating; Low copper erosion; Formation of stable intermetallic layer.
Physical Properties Metric English Comments
Specific Gravity 7.50 g/cc
7.50 g/cc
Mechanical Properties Metric English Comments
Tensile Strength 52.0 MPa
7540 psi
Elongation at Break 27 %
27 %
Thermal Properties Metric English Comments
Specific Heat Capacity 0.220 J/g-°C
0.0526 BTU/lb-°F
Thermal Conductivity 64.0 W/m-K
444 BTU-in/hr-ft²-°F
Melting Point 227 °C
441 °F
Component Elements Properties Metric English Comments
Copper, Cu 0.70 %
0.70 %
Germanium, Ge <= 0.010 %
<= 0.010 %
Nickel, Ni 0.050 %
0.050 %
Tin, Sn 99.25 %
99.25 %
As Remainder
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000150 ohm-cm
0.0000150 ohm-cm
Users viewing this material also viewed the following: