Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000150 ohm-cm | 0.0000150 ohm-cm | |
Nihon Superior SN100CL Lead-Free Solder Alloy Used for hot air solder leveling (HASL). Features include: Excellent fluidity; Bridge-free coating of the fine pitch circuitry; Bright smooth and uniform coating; Low copper erosion; Formation of st.. |
|||
Electrical Resistivity | 0.0000150 ohm-cm | 0.0000150 ohm-cm | |
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation. |
|||
Electrical Resistivity | 0.0000150 ohm-cm | 0.0000150 ohm-cm | |
Indium Corp. Indalloy 109 Tin-Lead Solder Alloy Good electrical grade solderInformation Provided by Indium Corporation |
|||
Electrical Resistivity | 0.0000150 ohm-cm | 0.0000150 ohm-cm | |
Indium Corp. Indalloy® 1E In-Sn Solder Alloy Lowest melting point practical solder. Indium-tin eutectic with sharp melting point. Has good wettability on glass, quartz and many ceramics. Has good low temperature malleability and therefore com.. |
|||
Electrical Resistivity | 0.0000150 ohm-cm | 0.0000150 ohm-cm | 3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02 |
California Fine Wire Nickel Alloy 90 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Electrical Resistivity | 0.0000150 ohm-cm | 0.0000150 ohm-cm | |
ATI Wah Chang Niobium Niobium is a soft, ductile metal which can be cold worked over 90 percent before annealing becomes necessary. In appearance, the metal is somewhat similar to stainless steel. The density of 8.57 gm/.. |