Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 137
137
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 108 cSt
108 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 15 cSt
15 cSt
Base Oil; ASTM D445
Evaporation Loss 0.10 %
0.10 %
24 hrs, 100C; ASTM D972
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Recommended
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Recommended
Pour Point -55.0 °C
-67.0 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type Pennzane