Nye Lubricants 702A-EP (NG) Synthetic Oil

Category Fluid , Lubricant , Silica Gellant
Manufacturer Nye Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 702A-EP (NG) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 65
65
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 220 cSt
220 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 15 cSt
15 cSt
Base Oil; ASTM D445
Evaporation Loss 1.0 %
1.0 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 260
260
ASTM D217
Penetration P(60), 1/10 mm 260
260
ASTM D217
Oil Separation 0.50 %
0.50 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 165 °C
329 °F
Recommended
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Recommended
Descriptive Properties Value Comments
Base Fluid Type Petroleum
Gellant Type Silica (WL)