Nye Lubricants 733MS (RL) Synthetic Oil

Category Fluid , Lubricant , Clay Gellant , Polyalphaolefin (PAO)
Manufacturer Nye Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 733MS (RL) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 127
127
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 32 cSt
32 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 5.4 cSt
5.4 cSt
Base Oil; ASTM D445
Evaporation Loss 12 %
12 %
22 hrs, 175C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 300
300
ASTM D217
Penetration P(60), 1/10 mm 315
315
ASTM D217
Oil Separation 10 %
10 %
22 hrs, 175C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Recommended
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Recommended
Pour Point -62.0 °C
-79.6 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PAO
Gellant Type Clay