Nylene® 734 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer Nylene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 734 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dry as molded. Injection molding grade. Nylene 734 is the heat stabilized version of 733 which is a high impact modified nylon suitable for both molding and extrusion. In addition to heat stabilization to prevent thermal degradation, parts molded from 734 have excellent impact strength right out of the mold without post conditioning. Outstanding features of Nylene 734 include high stiffness and high strength. Cylinder temperatures should be in the 500 - 550ºF range.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 72.0 MPa
10400 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 8.40 J/cm
15.7 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C
142 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 275 °C
527 °F