Nylene® Naxel™ PC40CV Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Nylene®
Trade Name Naxel™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Naxel™ PC40CV Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Naxel™ PC40CV is a 17 melt, virgin, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Melt Flow 17 g/10 min
17 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.7 MPa
8800 psi
ASTM D638
Elongation at Break 110 %
110 %
ASTM D638
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 6.94 J/cm
13.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
ASTM D648