Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® Vexel™ B12U FR Un-reinforced, Flame Retardant PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer Nylene®
Trade Name Vexel™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Vexel™ B12U FR Un-reinforced, Flame Retardant PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vexel™ B12U FR is an un-reinforced, flame retardant PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.016 cm/cm
0.010 - 0.016 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 49.0 MPa
7100 psi
ASTM D638
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 227 °C
440 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C
150 °F
ASTM D648
Users viewing this material also viewed the following: