Category Ceramic , Clay , Ball Clay
Manufacturer Old Hickory Clay Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Old Hickory M-33 Kentucky Ball Clay.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The M-33 ball clay is a carbonaceous selection that bears similarity to some clays found in the Southwestern section of England. It has a uniquely waxy type of plasticity and provides high green and dry strength to a variety of white ware ceramic formulations. especially sanitary ware. The organic content is largely of colloidal size, which offers the added advantage of rheology stability and ease of casting slip deflocculation. Due to this rich source of colloidal organic content, our M-33 should be considered as an additive type clay in percentages of 50% or less of the total ball clay content of white ware formula.Information provided by Old Hickory Clay Company
Physical Properties Metric English Comments
Particle Size 0.50 µm
0.50 µm
44% of particles less than
0.67 µm
0.67 µm
Median particle diameter
1.0 µm
1.0 µm
61% of particles less than
<= 5.0 µm
<= 5.0 µm
86% of particles less than
pH 6.3
6.3
Soluble Sulfates 230 ppm
230 ppm
Specific Surface Area 22.1 m²/g
22.1 m²/g
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00483 GPa
0.700 ksi
Dry Modulus of Rupture for 50% clay/50% flint, cast bars
Thermal Properties Metric English Comments
Shrinkage 5.2 %
5.2 %
Cone 04, Linear Fired Shrinkage
8.5 %
8.5 %
Cone 3, Linear Fired Shrinkage
9.0 %
9.0 %
Linear Drying Shrinkage
11.6 %
11.6 %
Cone 11, Linear Fired Shrinkage
Component Elements Properties Metric English Comments
Al2O3 24.98 %
24.98 %
CaO 1.69 %
1.69 %
Fe2O3 1.81 %
1.81 %
K2O 0.080 %
0.080 %
Loss on Ignition(%) 16.06 %
16.06 %
MgO 0.29 %
0.29 %
Na2O 0.61 %
0.61 %
SiO2 53.55 %
53.55 %
TiO2 1.69 %
1.69 %
Descriptive Properties Value Comments
Absorption (%) 1
Cone 11, Fired
13.5
Cone 04, Fired
6.2
Cone 3, Fired
CEC/MBI (meg/100 ml) 13.6
Crude Color Dark Brown
Filtration (ml) 14
Pyrometric Cone Equivalent (PCE) 31
Water of Plasticity (%) 38
Wet Sieve Residue (%) 3.29
Wet Sieve Residue, +200 mesh