Material Notes:
A beneficiated calcium carbonate with excellent fineness, color, and dispersion characteristics available in dry and slurry forms.Applications: Employed in rubber and plastic applications such as rigid PVC and plasticized PVC. Also used in all types of coatings and paints, putties, caulk, and sealants.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 1.85 g/cc
1.85 g/cc
Slurry
2.70 g/cc
2.70 g/cc
dry
Density 1.854 g/cc
0.06697 lb/in³
Slurry
Solids Content 72 %
72 %
Slurry
Brightness 95.5 %
95.5 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.040 %
0.040 %
Moisture Loss at 110°C % (dry)
Particle Size 3.2 µm
3.2 µm
Median Diameter
Specific Surface Area 3.2 m²/g
3.2 m²/g
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
dry
Descriptive Properties Value Comments
Calcium Carbonate % 98
FDA 21 CFR 174.5, 175.300, 178.3297
Hegman (dry) 6
Magnesium Carbonate % 1
Pounds Pigment/gallon (slurry) 11.3
Pounds Pigment/Solid Gallon (dry) 22.6
Retained in 325 mesh (dry) ppm 40