Material Notes:
A high purity, fine, wet ground natural calcium carbonate available in slurry form.Applications: Decorative paints.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 1.88 g/cc
1.88 g/cc
Density 1.876 g/cc
0.06779 lb/in³
Slurry
Solids Content 74 %
74 %
as Supplied
Brightness 96 %
96 %
Y - Brightness (dry)
Particle Size 1.4 µm
1.4 µm
Median Diameter
Specific Surface Area 7.0 m²/g
7.0 m²/g
Brookfield Viscosity 200 cP

@Temperature 25.0 °C
200 cP

@Temperature 77.0 °F
No. 3 Spindle, 100 rpm
Descriptive Properties Value Comments
Calcium Carbonate % 98
FDA 21 CFR 174.5, 175.300, 178.3297
Magnesium Carbonate % 1
Percent Finer than 1 Microns 40
Percent Finer than 2 Microns 60
Pounds Pigment/gallon (slurry) 11.59
Pounds Pigment/Solid Gallon (dry) 11.59
Retained in 325 mesh (dry) ppm 2