Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | BET |
Nabaltec NABALOX® NO 713-10 MF Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 7.0 - 9.0 m²/g | 7.0 - 9.0 m²/g | BET |
Nabaltec NABALOX® NO 713-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
Omya HYDROCARB® 60 Calcium Carbonate A fine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
Omya HYDROCARB® 60 HS Calcium Carbonate A fine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
Omya OMYACARB® F - FL Calcium Carbonate A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
Omya OMYAFIL® 60 Calcium Carbonate A fine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
Omya OMYAFLOW® F - SY Calcium Carbonate A high purity, fine, wet ground natural calcium carbonate available in slurry form.Applications: Decorative paints.Information supplied by Omya North America. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
Momentive Performance Materials HCPL Boron Nitride (BN) Powder All Grade HCP powders are high purity, fine (99%, -325 mesh), hexagonal Boron Nitride (BN). All exhibit the unique properties of BN in a form readily used in many advanced materials and processes. .. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
Momentive Performance Materials PolarTherm® PTX60 Boron Nitride (BN) Powder Spherical BN Agglomeration Powder. Spherical nature may improve thermal conductivity at moderate loading levels when used as a filler in polymers or lubricants, and produce less anisotropic propert.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
American Elements Antimony Nanoparticles General DescriptionAntimony (Sb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Antimony Particles are typically 20-40 nano.. |
|||
Specific Surface Area | 7.0 - 10 m²/g | 7.0 - 10 m²/g | |
American Elements Antimony Oxide Nanopowder General DescriptionAntimony Oxide ( SbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
American Elements Antimony Tin Oxide Nanoparticles General DescriptionAntimony Tin Oxide (ATO) Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. N.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
American Elements Barium Titanate nanoparticles General DescriptionBarium Titanate Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nanoscale .. |
|||
Specific Surface Area | 7.0 - 10 m²/g | 7.0 - 10 m²/g | |
American Elements Bismuth Oxide Nanopowder General DescriptionBismuth Oxide ( BiO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
American Elements Iron Cobalt Nanopowder General DescriptionIron Cobalt ( FeCo) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
American Elements Iron Nanoparticles General DescriptionIron (Fe) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Iron Particles are typically 20-40 nanometers (.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
American Elements Iron Nickel Nanopowder General DescriptionIron Nickel ( FeNi) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nano.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
American Elements Iron Oxide Nanopowder General DescriptionIron Oxide ( Fe2O3 and Fe3O4) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure part.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
American Elements Lead Oxide Nanopowder General DescriptionLead Oxide ( PbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Lead Oxide Par.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
American Elements Manganese Nanoparticles General DescriptionManganese (Mn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Manganese Particles are typically 20-40 na.. |
|||
Specific Surface Area | 7.0 - 10 m²/g | 7.0 - 10 m²/g | |
American Elements Molybdenum Oxide Nanopowder General DescriptionMolybdenum Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles... |
|||
Specific Surface Area | 7.0 - 10 m²/g | 7.0 - 10 m²/g | |
American Elements Niobium Oxide Nanoparticles General DescriptionNiobium Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Specific Surface Area | 7.0 - 10 m²/g | 7.0 - 10 m²/g | |
American Elements Tantalum Oxide Nanopowder General DescriptionTantalum Oxide ( TaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N.. |
|||
Specific Surface Area | 7.0 - 11 m²/g | 7.0 - 11 m²/g | |
DuPont™ Kevlar® Aramid Pulp Sold as highly fibrillated, short (0.5-1mm) fibers. Kevlar® pulps are chopped fibers that can be used as specialty additives to enhance performance by providing excellent reinforcement and viscos.. |
|||
Specific Surface Area | 7.0 - 12 m²/g | 7.0 - 12 m²/g | Nitrogen; ASTM D6556 |
Cancarb Thermax® Floform N907 Stainless Medium Carbon Black Thermal carbon black, often referred to as MT black, is unique in several ways. Along the carbon black spectrum, it has the largest particle size and among the lowest degrees of particle aggregation.. |
|||
Specific Surface Area | 7.0 - 12 m²/g | 7.0 - 12 m²/g | Nitrogen; ASTM D6556 |
Cancarb Thermax® Powder N908 Stainless Medium Carbon Black Thermal carbon black, often referred to as MT black, is unique in several ways. Along the carbon black spectrum, it has the largest particle size and among the lowest degrees of particle aggregation.. |
|||
Specific Surface Area | 7.0 m²/g | 7.0 m²/g | |
Momentive Performance Materials PolarTherm® PTX25 Boron Nitride (BN) Powder Spherical BN Agglomeration Powder. Spherical nature may improve thermal conductivity at moderate loading levels when used as a filler in polymers or lubricants, and produce less anisotropic propert.. |