Material Notes:
Nemcon E-series products are designed for use in ESDA electronic assembly environments where strict control of ESD and cleanliness are critical. Nemcon E PC 08CF is a carbon fiber-reinforced polycarbonate characterized by high stiffness, consistent moldability, low sloughing and uniform conductivity. ApplicationsShipping/handling trays for HDD components, ICs and display assembliesInternal components/assembliesCleanroom tools/test equipmentInformation provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 93.0 MPa
13500 psi
50 mm/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
50 mm/min; ASTM D638
Tensile Modulus 5.60 GPa
812 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 152 MPa
22000 psi
1.3 mm/min; ASTM D790
Flexural Modulus 6.40 GPa
928 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.694 J/cm

@Temperature 23.0 °C
1.30 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C

@Thickness 3.20 mm
275 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 72000 ohm
72000 ohm
ASTM D257