Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.40 GPa | 928 ksi | 1.3 mm/min; ASTM D790 |
Ovation Polymers Nemcon™ E PC 08CF Polycarbonate Nemcon E-series products are designed for use in ESDA electronic assembly environments where strict control of ESD and cleanliness are critical. Nemcon E PC 08CF is a carbon fiber-reinforced polyca.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Nilit FRIANYL A63 GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Nilit FRIANYL A63 HS-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | <= 6.40 GPa | <= 928 ksi | |
Reliance Industries Polypropylene - 30% glass fiber filled Information provided by Reliance Industries |
|||
Flexural Modulus | <= 6.40 GPa | <= 928 ksi | |
Reliance Industries Polypropylene - Suzorite mica (untreated) filler Information provided by Reliance Industries |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP CX05031 PS (Europe-Africa-Middle East) LNP* Lubricomp* CX05031 is a compound based on Polystyrene resin containing Graphite, Silicone. Added features include; Internally Lubricated. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ASTM D790 |
Shell Carilon® DB6F5G40 Polyketone, Flame-Retarded (V-0), 20% Glass-Reinforced Injection Molding Grade
(disco Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F5G40 is a flame-retarded, 20 percent glass-fiber-reinforced, injection molding grade with mecha.. |
|||
Flexural Modulus | 6.40 GPa @Temperature 60.0 °C |
928 ksi @Temperature 140 °F |
ASTM D790 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ASTM D790 |
LG Chemical LUCEL CF-610 Electrically Conductive POM, 10% Carbon Fiber Filled, High Strength, Wear Resistant LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Grupo Repol Dinalon® B1S25 G30 PA6 30% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178-A |
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber PA 6, 20% glass fiber, injection molding, heat-ageing stabilized, weather stabilized, improved surface finishInformation provided by LANXESS. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178-A |
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This .. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP (Europe-Africa-Middle East) LNP* Lubricomp* MFL36S is a compound based on Polypropylene resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East) 15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, DRY Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, Conditioned Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, DRY Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS (Asia Pacific) LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp ZF0041XC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF0041XC is a compound based on PPE+PS Blend resin containing Glass Fiber and Flame retardant. Added features include Flame Retardant.This data was supplied by SABIC-IP for the Euro.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Polyplastics FR-PET® BN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ASTM D790 |
Chem Polymer Chemlon 225 G Nylon 6, 25% Glass Fiber Reinforced A 25% glass fiber reinforced nylon 6 offering a balance of properties between the 20% (Chemlon 220 G) and 30% (Chemlon 233 G) product offerings. This product offers further improvements in tensile .. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 272 Polystyrene Alloy, Glass Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Asia Pacific) LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |