P & P Technology BeCu alloy 25 (CA172) Contact Finger Strips

Category Metal , Nonferrous Metal , Beryllium Alloy , Copper Alloy
Manufacturer P & P Technology
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF P & P Technology BeCu alloy 25 (CA172) Contact Finger Strips.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The CFS range of contact finger strips are available in Beryllium Copper, Phosphor Bronze and Stainless Steel. Many plating options are also available. Contact finger strips are used to close the aperture between two surfaces and provide high EMI shielding effectiveness. The strips are very versatile in applications where low closure force is required such as enclosures.Material Specification: (Beryllium Copper) BeCu alloy 25(CA172) is used for maximum spring, strength and fatigue resistance.Information provided by P & P Technology
Mechanical Properties Metric English Comments
Tensile Strength 175 - 185 MPa
25400 - 26800 psi
Heat Treated
Modulus of Elasticity 185 GPa
26800 ksi
Heat Treated
Component Elements Properties Metric English Comments
Beryllium, Be 1.8 - 2.0 %
1.8 - 2.0 %
Co + Ni >= 0.20 %
>= 0.20 %
Co + Ni + Fe >= 0.60 %
>= 0.60 %
Copper, Cu 97.2 %
97.2 %
Electrical Properties Metric English Comments
Volume Resistivity 0.00000769 - 0.0000080 ohm-cm
0.00000769 - 0.0000080 ohm-cm
Heat Treated
Shielding Effectiveness >= 110 dB

@Frequency 100000 Hz
>= 110 dB

@Frequency 100000 Hz
H-Field
>= 110 dB

@Frequency 1.00e+7 Hz
>= 110 dB

@Frequency 1.00e+7 Hz
E-Field
>= 110 dB

@Frequency 1.00e+9 Hz
>= 110 dB

@Frequency 1.00e+9 Hz
P-Field
Descriptive Properties Value Comments
Temper 1000 psi
Heat Treated