Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 110 dB @Thickness 1.60 mm, Frequency 1.00e+9 Hz |
110 dB @Thickness 0.0630 in, Frequency 1.00e+9 Hz |
MIL G83528 |
Rogers Corporation Bisco® EC-2130 Conductive Silicone Base Polymer: SiliconeFiller: Nickel-GraphiteApplications: Silicone EMI ShieldsThickness: 0.063 inches and 0.125 inchesInformation provided by Rogers Corporation. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 100000 Hz |
>= 110 dB @Frequency 100000 Hz |
H-Field |
P & P Technology BeCu alloy 25 (CA172) Contact Finger Strips The CFS range of contact finger strips are available in Beryllium Copper, Phosphor Bronze and Stainless Steel. Many plating options are also available. Contact finger strips are used to close the ap.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 1.00e+7 Hz |
>= 110 dB @Frequency 1.00e+7 Hz |
E-Field |
P & P Technology BeCu alloy 25 (CA172) Contact Finger Strips The CFS range of contact finger strips are available in Beryllium Copper, Phosphor Bronze and Stainless Steel. Many plating options are also available. Contact finger strips are used to close the ap.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 1.00e+9 Hz |
>= 110 dB @Frequency 1.00e+9 Hz |
P-Field |
P & P Technology BeCu alloy 25 (CA172) Contact Finger Strips The CFS range of contact finger strips are available in Beryllium Copper, Phosphor Bronze and Stainless Steel. Many plating options are also available. Contact finger strips are used to close the ap.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+10 Hz |
110 dB @Frequency 1.00e+10 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology ECF-J Silver Aluminum Loaded Fluorosilicone P & P Technology material reference ECF-J is a fluorosilicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical pro.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+10 Hz |
110 dB @Frequency 1.00e+10 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology EC-H Silver Copper Loaded Fluorosilicone P & P Technology material reference EC-H is a printing grade fluorosilicone elastomer with a Silver/Copper conductive filler and is green in color. The material is specially compounded to offer exc.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+10 Hz |
110 dB @Frequency 1.00e+10 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology EC-H Silver Copper Loaded Silicone P & P Technology material reference EC-H is a printing grade silicone elastomer with a Silver/Copper conductive filler and is Tan in color. The material is specially compounded to offer excellent p.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+10 Hz |
110 dB @Frequency 1.00e+10 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology EC-J Silver Aluminum Loaded Silicone P & P Technology material reference EC-J is a silicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical properties.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 1.00e+8 Hz |
>= 110 dB @Frequency 1.00e+8 Hz |
E Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1239 Conductive Elastomer Material for waveguide choke, cover, and flange EMI shielding and pressure sealing; maximum heat transfer and minimum outgassing; hard (80 Shore A), high-strength material; available with raised lip.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 5.00e+8 Hz |
>= 110 dB @Frequency 5.00e+8 Hz |
E Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1239 Conductive Elastomer Material for waveguide choke, cover, and flange EMI shielding and pressure sealing; maximum heat transfer and minimum outgassing; hard (80 Shore A), high-strength material; available with raised lip.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 2.00e+9 Hz |
>= 110 dB @Frequency 2.00e+9 Hz |
Plane Wave; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1239 Conductive Elastomer Material for waveguide choke, cover, and flange EMI shielding and pressure sealing; maximum heat transfer and minimum outgassing; hard (80 Shore A), high-strength material; available with raised lip.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 1.00e+10 Hz |
>= 110 dB @Frequency 1.00e+10 Hz |
Plave Wave; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1239 Conductive Elastomer Material for waveguide choke, cover, and flange EMI shielding and pressure sealing; maximum heat transfer and minimum outgassing; hard (80 Shore A), high-strength material; available with raised lip.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 5.00e+8 Hz |
>= 110 dB @Frequency 5.00e+8 Hz |
E Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1285 Conductive Elastomer Conductive Elastomer with Improved Corrosion Resistance. This conductive silicone elastomer features significantly improved corrosion resistance in salt spray environments over silver-plated copper-.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 1.00e+8 Hz |
>= 110 dB @Frequency 1.00e+8 Hz |
E Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 1.00e+8 Hz |
>= 110 dB @Frequency 1.00e+8 Hz |
E Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 2.00e+9 Hz |
>= 110 dB @Frequency 2.00e+9 Hz |
Plane Wave; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 6503 Conductive Elastomer Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 2.00e+9 Hz |
>= 110 dB @Frequency 2.00e+9 Hz |
Plane Wave; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 6510 Conductive Elastomer Extruded onlyInformation provided by Chomerics |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+8 Hz |
110 dB @Frequency 1.00e+8 Hz |
|
Parker Chomerics SOFT-SHIELD® 5000 Low Closure Force EMI Gasket Description: SOFT-SHIELD® 5000 Series EMI gaskets are designed to meet the stringent shielding and mechanical performance requirements of today’s commercial electronic enclosures, medical electron.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+10 Hz |
110 dB @Frequency 1.00e+10 Hz |
|
Parker Chomerics SOFT-SHIELD® 5000 Low Closure Force EMI Gasket Description: SOFT-SHIELD® 5000 Series EMI gaskets are designed to meet the stringent shielding and mechanical performance requirements of today’s commercial electronic enclosures, medical electron.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+10 Hz |
110 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Waveguide Gaskets 877 Conductive Silicone Elastomer Gasket Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.Application Information: TECKNIT W.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+9 Hz |
110 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-A 895 Silver-Aluminum Filled Silicone Elastomer Description: CONSIL-A is a silicone or fluorosilicone elastomer filled with silver-plated aluminum particles designed to achieve maximum electrical conductivity. CONSIL-A provides high shielding eff.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+7 Hz |
110 dB @Frequency 1.00e+7 Hz |
E-Field |
Parker Chomerics Tecknit Consil®-A 897 Silver-Aluminum Filled Silicone Elastomer Description: CONSIL-A is a silicone or fluorosilicone elastomer filled with silver-plated aluminum particles designed to achieve maximum electrical conductivity. CONSIL-A provides high shielding eff.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+10 Hz |
110 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-C 871 Silver-Copper Filled Silicone Elastomer Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+10 Hz |
110 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-C 873 Silver-Copper Filled Silicone Elastomer Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+10 Hz |
110 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-C 875 Silver-Copper Filled Silicone Elastomer Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+9 Hz |
110 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-N 891 Silver-Nickel Filled Silicone Elastomer Description: CONSIL-N is a silicone elastomer filled with silver-plated nickel particles and designed to provide high shielding effectiveness and corrosion resistance. CONSIL-N is available in sheet.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 1.00e+10 Hz |
>= 110 dB @Frequency 1.00e+10 Hz |
E Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1217 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |
|||
Shielding Effectiveness | >= 110 dB @Frequency 2.00e+9 Hz |
>= 110 dB @Frequency 2.00e+9 Hz |
Plane Wave; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 6502 Conductive Elastomer Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric.. |
|||
Shielding Effectiveness | 110 dB @Frequency 1.00e+10 Hz |
110 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Waveguide Gaskets 873 Conductive Silicone Elastomer Gasket Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.Application Information: TECKNIT W.. |
|||
Shielding Effectiveness | 110 dB @Thickness 0.508 mm, Frequency 1.00e+9 Hz |
110 dB @Thickness 0.0200 in, Frequency 1.00e+9 Hz |
MIL G83528 |
Rogers Corporation Bisco® EC-2040 Conductive Silicone Base Polymer: SiliconeFiller: Nickel-GraphiteApplications: Silicone EMI ShieldsThickness: 0.020 inches and 0.031 inchesInformation provided by Rogers Corporation. |