PB1000-650 Polyurethane-based Biomedical Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PB1000-650 Polyurethane-based Biomedical Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 75
65 - 75
ASTM D2240
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D412
Tensile Strength, Yield 36.5 MPa
5300 psi
at 100%; ASTM D412
Elongation at Break 350 %
350 %
ASTM D412