Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PCP-Canada ALCA 5® 5083 Cast Aluminum Mold Plate

Category Metal , Nonferrous Metal , Aluminum Alloy , Aluminum Casting Alloy
Manufacturer PCP-Canada
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PCP-Canada ALCA 5® 5083 Cast Aluminum Mold Plate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ALCA5® cast precision plate product has an excellent dimensional stability. The low level of internal stress reduces the plate deformation during and after machining. This high stability leads to cost saving on extra operations such as rough-milling, finishing or re-works. Typical applications are reference plates, machine construction, molds, jigs, and construction equipments.Information provided by PCP-Canada.
Physical Properties Metric English Comments
Density 2.66 g/cc
0.0960 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 70
70
Tensile Strength, Ultimate 283 MPa
41000 psi
Tensile Strength, Yield 124 MPa
18000 psi
Elongation at Break 16 %
16 %
in 2 inches
Modulus of Elasticity 71.0 GPa
10300 ksi
Thermal Properties Metric English Comments
CTE, linear 23.8 µm/m-°C

@Temperature 20.0 - 100 °C
13.2 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 120 W/m-K
832 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Aluminum, Al 92.55 - 95.55 %
92.55 - 95.55 %
as remainder
Chromium, Cr 0.050 - 0.25 %
0.050 - 0.25 %
Copper, Cu <= 0.10 %
<= 0.10 %
Iron, Fe <= 0.40 %
<= 0.40 %
Magnesium, Mg 4.0 - 4.9 %
4.0 - 4.9 %
Manganese, Mn 0.40 - 1.0 %
0.40 - 1.0 %
Other <= 0.15 %
<= 0.15 %
Ti + Zr
Silicon, Si <= 0.40 %
<= 0.40 %
Zinc, Zn <= 0.25 %
<= 0.25 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000640 ohm-cm
0.00000640 ohm-cm
Users viewing this material also viewed the following: