Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 23.8 µm/m-°C | 13.2 µin/in-°F | ASTM D696-08 |
Haysite H208 Polyester, Magnetic Permeable Grade H208 has high magnetic permeability and excellent retention of properties after heat aging at elevated temperatures. This unique combination of properties allows Grade H208 to be used in vari.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
PCP-Canada ALCA 5® 5083 Cast Aluminum Mold Plate ALCA5® cast precision plate product has an excellent dimensional stability. The low level of internal stress reduces the plate deformation during and after machining. This high stability leads to c.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
average |
Alcoa UltrAlloy® 6020-T651 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
average |
Alcoa UltrAlloy® 6020-T8 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
average |
Alcoa UltrAlloy® 6020-T9 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium Alumold® 110 Aluminum Cast Sliced Plate Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma.. |
|||
CTE, linear | 23.7 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
CTE, linear | 23.7 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
CTE, linear | 23.7 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium Fibral® Cast Aluminum Sliced Plate Fibral® has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The materia.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium Formall® 545 Aluminum Alloy Formall®-545 is a super plastically formable alloy. Both chemical composition and processing conditions have been developed for optimum superplastic behavior and to guarantee the advantages of an a.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium PLAN 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium PLAN OX 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Alpase K100-S™ Aluminum Plate K100-S™ features and benefits include: Dimensional stability, fully weldable, anodizable, high elongation, consistent properties - regardless of size, close flatness and tolerances, superior corros.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
AA 5005 |
Aleris 55HX® Aluminum (5005-H14) Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ.. |
|||
CTE, linear | 23.8 µm/m-°C @Temperature 20.0 - 100 °C |
13.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
PCP-Canada Max 5® 5083 Cast Aluminum Mold Block Max 5® is characterized by an excellent dimensional stability. It is a 5083 alloy which provides strength, good hard anodizing response, weldability, and machinability (with sintered carbide materi.. |