Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PCP-Canada Max 5® 5083 Cast Aluminum Mold Block

Category Metal , Nonferrous Metal , Aluminum Alloy , Aluminum Casting Alloy
Manufacturer PCP-Canada
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PCP-Canada Max 5® 5083 Cast Aluminum Mold Block.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Max 5® is characterized by an excellent dimensional stability. It is a 5083 alloy which provides strength, good hard anodizing response, weldability, and machinability (with sintered carbide materials). Easy to recycle with high residual value at the end of its useful life. Internal low level of MAX5® porosity is guaranteed by the supplier casting technology. Quality control is made by ultrasonic inspection. The low density of the 5000 series is an advantage over other aluminum mold products.Information provided by PCP-Canada.
Physical Properties Metric English Comments
Density 2.66 g/cc
0.0960 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 70
70
Tensile Strength, Ultimate 283 MPa
41000 psi
Tensile Strength, Yield 124 MPa
18000 psi
Elongation at Break 16 %
16 %
in 2 inches
Modulus of Elasticity 71.0 GPa
10300 ksi
Thermal Properties Metric English Comments
CTE, linear 23.8 µm/m-°C

@Temperature 20.0 - 100 °C
13.2 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 120 W/m-K
832 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Aluminum, Al 92.55 - 95.55 %
92.55 - 95.55 %
as remainder
Chromium, Cr 0.050 - 0.25 %
0.050 - 0.25 %
Copper, Cu <= 0.10 %
<= 0.10 %
Iron, Fe <= 0.40 %
<= 0.40 %
Magnesium, Mg 4.0 - 4.9 %
4.0 - 4.9 %
Manganese, Mn 0.40 - 1.0 %
0.40 - 1.0 %
Other <= 0.15 %
<= 0.15 %
Ti + Zr
Silicon, Si <= 0.40 %
<= 0.40 %
Zinc, Zn <= 0.25 %
<= 0.25 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000640 ohm-cm
0.00000640 ohm-cm
Users viewing this material also viewed the following: