Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PSM Industries Ferro-TiC® PK Maraging Steel

Category Ceramic , Carbide , Metal , Ferrous Metal , Maraging Steel
Manufacturer PSM Industries
Trade Name Ferro-TiC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries Ferro-TiC® PK Maraging Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Combination of excellent transverse rupture strength, impact strength, and corrosion resistance. Good thermal shock resistance. Magnetic.Ferro-TiC® Unique CharacteristicsProvides the lightweight, size, stability, and hardnessVirtually porosity free - significantly better than the A1 ASTM B-276-79 StandardLow specific mass. Ferro-Tic® is 10-20% lighter than its steel counterpart and about 50% lighter than tungsten carbide10 times the wear resistance of tool steelsEconomical fabrication (conventionally machinable in the annealed stage by milling and turning, conventionally heat treatable to achieve high hardness)50-90% less linear size change in heat treat than tool steelsInformation Provided by Ferro-TiC®, a division of PSM Industries
Physical Properties Metric English Comments
Density 6.60 g/cc
0.238 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 50
50
Annealed
61
61
Hardened
Flexural Strength 1380 MPa
200000 psi
Transverse Rupture
Compressive Strength 2880 MPa
417000 psi
Charpy Impact Unnotched 7.367 J/cm²
35.08 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear 3.80 µm/m-°C

@Temperature 21.1 - 449 °C
2.11 µin/in-°F

@Temperature 70.0 - 840 °F
Maximum Service Temperature, Air 449 °C
840 °F
Descriptive Properties Value Comments
Carbide (Vol. %) 42
Linear Size Change Thru Heat Treat % -0.029
Thermal Shock (No. Cycles) 84
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved