Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.60 g/cc | 0.238 lb/in³ | |
PSM Industries Ferro-TiC® PK Maraging Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Comb.. |
|||
Density | 6.60 g/cc | 0.238 lb/in³ | |
MarkeTech Zirconium Oxide Ceramic - Zirconia, Y2O3 Stabilized Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is .. |
|||
Density | 6.60 g/cc | 0.238 lb/in³ | |
Indium Corp. Indalloy 176 Zinc Solder Alloy Information Provided by Indium Corporation |
|||
Density | 6.60 - 7.20 g/cc | 0.238 - 0.260 lb/in³ | |
China Tungsten ST2170 PM Antifriction Parts Information provided by China Tungsten |
|||
Density | 6.60 g/cc | 0.238 lb/in³ | Sintered |
Ametek P316L P/M Stainless Steel, Sintered from 6.30 g/cc Green Density P316L offers a very high degree of corrosion protection for a standard P/M stainless steel grade. It provides excellent strength at extremely high temperatures. Key materials benefits of P316L inclu.. |
|||
Density | 6.60 g/cc | 0.238 lb/in³ | |
Ametek P304L P/M Stainless Steel, Sintered from 6.5 g/cc Green Density Powder apparent bulk density 2.7 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for .. |
|||
Density | 6.60 g/cc | 0.238 lb/in³ | |
PSM Industries Ferro-TiC® C Medium Alloy Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Exce.. |
|||
Density | 6.60 g/cc | 0.238 lb/in³ | |
Ametek P303L P/M Stainless Steel, Sintered from 6.5 g/cc Green Density Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearate. Sintering was done in dissociated ammonia at 1121°C (2050°F) for .. |