Material Notes:
Information provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
24 hours at 73°F; ASTM D570
Melt Flow 6.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
6.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 58.6 MPa

@Thickness 3.17 mm
8500 psi

@Thickness 0.125 in
ASTM D638
Elongation at Break 100 %

@Thickness 3.17 mm
100 %

@Thickness 0.125 in
ASTM D638
Flexural Yield Strength 89.6 MPa

@Thickness 3.17 mm
13000 psi

@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.21 GPa

@Thickness 3.17 mm
321 ksi

@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 7.47 J/cm

@Thickness 3.17 mm
14.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ASTM D648