Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives TURBO-LOCK SERIES 13-OR Anaerobic Thread Locking Compound

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO-LOCK SERIES
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives TURBO-LOCK SERIES 13-OR Anaerobic Thread Locking Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TURBO-LOCK 13-OR SERIES is a RED, high temperature, high strength, permanent, oil resistant, anaerobic thread-locking compound. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals. Disassembles with high heat and hand toolsApplications:Ideal for applications where the temperatures range from -65 to 450ºF.Ideal for thread locking heavy duty applications such as bolts up to ¾” (20 mm) used in transmission, construction equipment or railroad assemblies, etc.Lubricated for easy assembly. Prevents loosening and leakage of threaded fasteners. Locks and seals threaded joints-nuts, screws, and studs. To disassemble, apply high heat and use tools.Part Numbers for this data: 13-000-OR, 13-001-OR, 13-010-OR, 13-050-OR, 13-250-OR, 13-1000-ORInformation provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Brookfield Viscosity 3750 cP
3750 cP
RVT Spindle 3 @ 20 rpm
Mechanical Properties Metric English Comments
Shear Strength 8.00 - 12.0 MPa
1160 - 1740 psi
Thermal Properties Metric English Comments
Flash Point >= 35.0 °C
>= 95.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 180 min
1.00 - 3.00 hour
Functional
1440 min
24.0 hour
Full
19.8 - 40.2 min

@Temperature -65.0 - 450 °C
0.330 - 0.670 hour

@Temperature -85.0 - 842 °F
Handling
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Red/Orange
Chemical Resistance 100% Initial Strength Retained
Acetone at 22°C, at 500hrs
100% Initial Strength Retained
Ethanol at 22°C, at 500hrs
100% Initial Strength Retained
Motor Oil at 125°C, at 500hrs
100% Initial Strength Retained
Gasoline at 22°C, at 500hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 500hrs
100% Initial Strength Retained
Ethanol at 22°C, at 1000hrs
100% Initial Strength Retained
Motor Oil at 125°C, at 1000hrs
100% Initial Strength Retained
Gasoline at 22°C, at 1000hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 1000hrs
80% Initial Strength Retained
Water/Glycol at 87°C, at 1000hrs
90% Initial Strength Retained
Water/Glycol at 87°C, at 500hrs
90% Initial Strength Retained
Acetone at 22°C, at 1000hrs
Composition Methacrylate Ester
Max Screw Size ¾” / 20 mm
Torque 25-35 N.m
Breakloose
25-35 N.m
Locking, Break
6-11 N.m
Locking, Prevailing
Users viewing this material also viewed the following: