Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives TURBO-LOCK SERIES 17-GP Anaerobic Thread Locking Compound

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO-LOCK SERIES
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives TURBO-LOCK SERIES 17-GP Anaerobic Thread Locking Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BEARING AND SHAFT - SERIES 17-GP is a fast curing, GREEN, high strength, general purpose, press fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals.Applications:Ideal to fill gaps up to 0.005” Excellent for press fitting parts. Withstands working temperatures up to 300ºFRetaining sleeves, pulleys, gears, rotors and fans on shafts.Mounting sleeves, securing bushings, bearings and plugs in housing.Excellent retaining and sealing compoundPart Numbers for this data: 17-001-GP, 17-010-GP, 17-050-GP, 17-250-GP, 17-1000-GPInformation provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Brookfield Viscosity 125 cP
125 cP
RVT Spindle 3 @ 20 rpm
Mechanical Properties Metric English Comments
Shear Strength 13.0 - 15.0 MPa

@Temperature 22.0 °C,
Time 108000 sec
1890 - 2180 psi

@Temperature 71.6 °F,
Time 30.0 hour
ISO 10123; Compressive, Steel pins and collars
17.0 - 19.0 MPa

@Temperature 22.0 °C,
Time 86400 sec
2470 - 2760 psi

@Temperature 71.6 °F,
Time 24.0 hour
ISO 10123; Compressive, Steel pins and collars
Thermal Properties Metric English Comments
CTE, linear 0.800 µm/m-°C
0.444 µin/in-°F
ASTM D696
Specific Heat Capacity 0.300 J/g-°C
0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Flash Point 37.8 °C
100 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 180 min
1.00 - 3.00 hour
Functional
1440 min
24.0 hour
Full
10.0 min

@Temperature -55.0 - 150 °C
0.167 hour

@Temperature -67.0 - 302 °F
Handling
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Green
Chemical Resistance 100% Initial Strength Retained
Acetone at 22°C, at 500hrs
100% Initial Strength Retained
Ethanol at 22°C, at 500hrs
100% Initial Strength Retained
Motor Oil at 125°C, at 500hrs
100% Initial Strength Retained
Gasoline at 22°C, at 500hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 500hrs
100% Initial Strength Retained
Ethanol at 22°C, at 1000hrs
100% Initial Strength Retained
Motor Oil at 125°C, at 1000hrs
100% Initial Strength Retained
Gasoline at 22°C, at 1000hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 1000hrs
80% Initial Strength Retained
Water/Glycol at 87°C, at 1000hrs
90% Initial Strength Retained
Water/Glycol at 87°C, at 500hrs
90% Initial Strength Retained
Acetone at 22°C, at 1000hrs
Composition Methacrylate Ester
Gap Fill 0.005"
Users viewing this material also viewed the following: