Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Panjin Zhongrun Chemerize 012P High Viscosity CoPEEK

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer Panjin Zhongrun High Performance Polymer Company
Trade Name Chemerize
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Panjin Zhongrun Chemerize 012P High Viscosity CoPEEK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Bieglo Gmbh.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0070 - 0.012 cm/cm
0.0070 - 0.012 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength 95.0 MPa
13800 psi
ISO 527
Elongation at Break 50 %
50 %
ISO 527
Flexural Strength 155 MPa
22500 psi
ISO 178
Flexural Modulus 3.70 GPa
537 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ISO 180/A
Izod Impact, Unnotched (ISO) NB
NB
ISO 180/U
Thermal Properties Metric English Comments
Melting Point >= 340 °C
>= 644 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 153 °C
307 °F
ISO75A
Flammability, UL94 V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ISO 60093
Dielectric Constant 3.2

@Frequency 1000 Hz
3.2

@Frequency 1000 Hz
ISO 60250
Dissipation Factor 0.0033

@Frequency 1000 Hz
0.0033

@Frequency 1000 Hz
ISO 60250
Descriptive Properties Value Comments
Form Pellets
Copyright © lookpolymers.com All Rights Reserved