Parker Chomerics CHO-FLEX 602 Conductive Coating

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer Parker Chomerics
Trade Name CHO-FLEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-FLEX 602 Conductive Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHO-FLEX™ 602 is a two-component silver-filled polyurethane coating designed for room temperature or oven cure. CHOFLEX™ 602 coating can be sprayed on large panels, cured at room temperature and coated with most military grade urethane or epoxy top coats. It can also be sprayed on most thermoplastic enclosures such as PPO, ABS, polystyrene and polycarbonate.Information provided by Chomerics
Physical Properties Metric English Comments
Density 2.10 g/cc
0.0759 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 107 °C
225 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.060 ohm
<= 0.060 ohm
Shielding Effectiveness 60 - 70 dB

@Frequency 1.00e+8 - 1.00e+9 Hz
60 - 70 dB

@Frequency 1.00e+8 - 1.00e+9 Hz
on epoxy/glass or epoxy/graphite
Processing Properties Metric English Comments
Cure Time 10100 min

@Temperature 25.0 °C
168 hour

@Temperature 77.0 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Binder Polyurethane
Consistency Thixotropic Paste
Filler Ag
Mix Ratio 100:13
Theoretical Coverage 4320 in2 / lb
Actual coverage will be 50-100%
Users viewing this material also viewed the following: