Material Notes:
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 2.45 - 2.95 g/cc
2.45 - 2.95 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 28 - 42
28 - 42
Tensile Strength at Break >= 0.552 MPa
>= 80.0 psi
ASTM D412
Tear Strength 3.50 kN/m
20.0 pli
Compression Set 80 %
80 %
70 hrs @ 100°C; ASTM D395 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 - 200 °C
320 - 392 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.033 ohm-cm
0.033 ohm-cm
as supplied without pressure sensitive adhesive
Shielding Effectiveness >= 60 dB
>= 60 dB
200 kHz (H Field); MIL-G-83528
>= 80 dB
>= 80 dB
10 GHz (Plane Wave); MIL-G-83528
>= 90 dB
>= 90 dB
2 GHz (Plane Wave); MIL-G-83528
>= 100 dB
>= 100 dB
100 MHz (E Field); MIL-G-83528
>= 100 dB
>= 100 dB
500 MHz (E Field); MIL-G-83528
Descriptive Properties Value Comments
Binder Silicone
EMP Survivability kA / in, min 0.3
Filler Ag
Vibration Resistance, After, ohm-cm max 0.03