Material Notes:
Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in the range of 70-80 dB, along with lower closure force, lower compression set and up to 20% lower cost than fabric-over-foam gaskets.Product Application: Panel seals, Cover seals, Grounding pads, Door seals, Desktop/laptop computers, Entertainment systems, CD/Receiver head units, Roadside Assistance systems and Satellite radio receivers.Information provided by Chomerics
Physical Properties Metric English Comments
Deformation 5.0 %
5.0 %
65 mOhm/sq in, at .05 in/min, 1 sq in area sample, 1mm
5.0 %
5.0 %
50 mOhm/sq in, at .05 in/min, 1 sq in area sample, 3mm
5.0 %
5.0 %
70 mOhm/sq in, at .05 in/min, 1 sq in area sample, 5mm
15 %
15 %
20 mOhm/sq in, at .05 in/min, 1 sq in area sample, 1mm
15 %
15 %
30 mOhm/sq in, at .05 in/min, 1 sq in area sample, 3mm
15 %
15 %
60 mOhm/sq in, at .05 in/min, 1 sq in area sample, 5mm
30 %
30 %
22 mOhm/sq in, at .05 in/min, 1 sq in area sample, 1mm
30 %
30 %
30 mOhm/sq in, at .05 in/min, 1 sq in area sample, 3mm
30 %
30 %
50 mOhm/sq in, at .05 in/min, 1 sq in area sample, 5mm
45 %
45 %
19 mOhm/sq in, at .05 in/min, 1 sq in area sample, 1mm
45 %
45 %
25 mOhm/sq in, at .05 in/min, 1 sq in area sample, 3mm
45 %
45 %
60 mOhm/sq in, at .05 in/min, 1 sq in area sample, 5mm
25 %

@Pressure 0.0172 MPa
25 %

@Pressure 2.50 psi
ASTM C165 Mod
50 %

@Pressure 0.0296 MPa
50 %

@Pressure 4.30 psi
ASTM C165 Mod
Mechanical Properties Metric English Comments
Tensile Strength 0.0683 MPa

@Thickness 3.00 mm
9.90 psi

@Thickness 0.118 in
ASTM D412
Compression Set <= 15 %
<= 15 %
Gasket; ASTM D3574
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Shielding Effectiveness 65 dB

@Frequency 1.00e+10 Hz
65 dB

@Frequency 1.00e+10 Hz
4mm x 6mm
65 dB

@Frequency 1.00e+10 Hz
65 dB

@Frequency 1.00e+10 Hz
5mm x 5mm
70 dB

@Frequency 1.00e+10 Hz
70 dB

@Frequency 1.00e+10 Hz
2mm x 6mm
75 dB

@Frequency 1.00e+10 Hz
75 dB

@Frequency 1.00e+10 Hz
1mm x 6mm
75 dB

@Frequency 1.00e+8 Hz
75 dB

@Frequency 1.00e+8 Hz
4mm x 6mm
70 - 80 dB

@Frequency 2.00e+7 - 1.00e+10 Hz
70 - 80 dB

@Frequency 2.00e+7 - 1.00e+10 Hz
CHO-TM-TP08
78 dB

@Frequency 1.00e+8 Hz
78 dB

@Frequency 1.00e+8 Hz
5mm x 5mm
79 dB

@Frequency 1.00e+9 Hz
79 dB

@Frequency 1.00e+9 Hz
5mm x 5mm
80 dB

@Frequency 1.00e+9 Hz
80 dB

@Frequency 1.00e+9 Hz
1mm x 6mm
80 dB

@Frequency 1.00e+9 Hz
80 dB

@Frequency 1.00e+9 Hz
2mm x 6mm
81 dB

@Frequency 1.00e+8 Hz
81 dB

@Frequency 1.00e+8 Hz
2mm x 6mm
82 dB

@Frequency 1.00e+8 Hz
82 dB

@Frequency 1.00e+8 Hz
1mm x 6mm
88 dB

@Frequency 1.00e+9 Hz
88 dB

@Frequency 1.00e+9 Hz
4mm x 6mm
Descriptive Properties Value Comments