Material Notes:
Comments: Thin flexible pasteTypical Applications: Bonding elastomer gasketInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 4.00 g/cc
4.00 g/cc
Volatile Organic Compounds (VOC) Content 285 g/l
285 g/l
Thickness 254 microns
10.0 mil
Mechanical Properties Metric English Comments
Shear Strength >= 0.345 MPa
>= 50.0 psi
Electrical Properties Metric English Comments
Volume Resistivity <= 0.010 ohm-cm
<= 0.010 ohm-cm
Processing Properties Metric English Comments
Cure Time 10100 min

@Temperature 24.0 °C
168 hour

@Temperature 75.2 °F
Shelf Life 9.00 Month
9.00 Month
Descriptive Properties Value Comments
Filler Ni
Mix Ratio 100:2.53
Resin System Silicone
Work Life 240 min
Users viewing this material also viewed the following: