Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pasargad Polymer Peyvand Pasalen 3P-M3520B Polypropylene, 20% EPDM Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Pasargad Polymer Peyvand
Trade Name Pasalen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pasargad Polymer Peyvand Pasalen 3P-M3520B Polypropylene, 20% EPDM Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components BumperAutomotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Polymer Peyvand Co
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.0 MPa
2760 psi
ISO 527-2
Elongation at Break >= 100 %
>= 100 %
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched NB
NB
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
Unannealed; ISO 75-2/C
Descriptive Properties Value Comments
Color Black