Pau Tai Dibasic lead stearate, Monomer Stabilizer

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Pau Tai Industrial Corp.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pau Tai Dibasic lead stearate, Monomer Stabilizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent lubricant at high temperature operation.Applications: Plate, injection molding products.
Physical Properties Metric English Comments
Specific Gravity 2.00 g/cc
2.00 g/cc
Particle Mesh Size 325 Mesh
325 Mesh
99.7%
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
Appearance White micropowder
Metal Content % 50+/- 1%