Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Premix Premi-Glas® 2550® CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas 2550® CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generation .. |
|||
Specific Gravity | 2.00 - 2.20 g/cc | 2.00 - 2.20 g/cc | ASTM D792 |
P & P Technology ECF-J Silver Aluminum Loaded Fluorosilicone P & P Technology material reference ECF-J is a fluorosilicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical pro.. |
|||
Specific Gravity | >= 2.00 g/cc | >= 2.00 g/cc | |
Parker Chomerics CHO-BOND 1067 Splicing Compound Kit Information provided by Chomerics |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Parker Chomerics Tecknit® 0036 Two Part Flexible Adhesive-Sealant Silver-Glass Silicone Description: TECKNIT 0036 is an electrically conductive, medium viscosity, RTV silicone adhesive-sealant. This silver-plated glass filled system is formulated with a special conductive material pro.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D4894 |
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Specific Gravity | 2.00 - 2.10 g/cc | 2.00 - 2.10 g/cc | ASTM D792 |
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 555 Perfluoroelastomer With its broad chemical resistance, Chemraz® 555, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. Chemraz 555 provides a significantly wider operational band.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D792 |
Spartech Sound X Noise Abatement Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Silberline Aquavet® 190nl-136M Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Silberline Aquavet® 205-136M Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D-792 |
Saint-Gobain Norton® F510 General Purpose Skived PTFE Sheet Description: PTFE = polytetrafluoroethyleneApplications include: General Purpose; Common in Electrical/ElectronicsInformation provided by Saint Gobain Performance Products. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
3M Dyneon™ 81TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 81TZ is a technically advanced high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per .. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Aremco Graphi-Coat™ 623 High Temperature Specialty Coatings Inorganic, Titanium Diboride Filled This coating system, originally patented by Aremco, is a tow-part, silica-bonded, titanium diboride filled, oxidation resistant coating for protecting graphite from oxidation to 2000°F (1093°C). U.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
3M Dyneon™ PFE 4131TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 4131TZ is an incorporated cure high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per .. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
3M Dyneon™ PFE 80Z Peroxide Cure Perfluoroelastomer 3M™ Dyneon™ Peroxide Cure Perfluoroelastomer PFE 80Z is a technically advanced peroxide curable perfluoroelastomer. This product is designed to have improved acid resistance and lower metal ion ex.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D792 |
3M Dyneon™ THV 500GZ Fluorothermoplastic Granules THV 500G is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provides a balance of low temperature proce.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Bulk Molding Compounds BMC 8005 Polyester Molding Compound |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | Part A; TM R050-16 |
Resinlab® EP1200 Black Casting Resin Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Resinlab® EP1285HD-10 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |