Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Permabond ET536 Epoxy Resin

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond ET536 Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PERMABOND ET536 is a two-part, 1:1 mixable epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET536 forms tough bonds providing high peel resistance and high shear strength. The extended work life of this product allows for adjustment and makes it more suitable for larger applications. Features & Benefits: Adhesion to a wide variety of substrates Full cure at room temperature Easy to apply High shear and peel strength Good impact strength Good chemical resistance Non-drip rheology Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ET536B, Polyamine Hardener
1.15 g/cc
1.15 g/cc
ET536A, Epoxy Resin
Viscosity 80000 cP

@Temperature 25.0 °C
80000 cP

@Temperature 77.0 °F
ET536A, Epoxy Resin
500000 cP

@Temperature 25.0 °C
500000 cP

@Temperature 77.0 °F
ET536B, Polyamine Hardener
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Elongation at Break 10 %
10 %
Adhesive Bond Strength 15.0 - 24.0 MPa
2180 - 3480 psi
Mild steel, Shear
Peel Strength 2.40 - 3.20 kN/m
13.7 - 18.3 pli
ISO 4578
Thermal Properties Metric English Comments
Thermal Conductivity 0.550 W/m-K
3.82 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 45.0 °C
113 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 90.0 min
1.00 - 1.50 hour
handling time
4320 min
72.0 hour
full cure
Pot Life 30.0 - 45.0 min

@Temperature 20.0 °C
30.0 - 45.0 min

@Temperature 68.0 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Black for Polyamine Hardener
White for Epoxy Resin
Maximum Gap Fill (mm) 5
Strength Retention 10% at 150°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C
Users viewing this material also viewed the following: